Step 1: Prepare materials: A:B:C=3:1:1
A:3KG (light yellow transparent)
B:1KG (white transparent)
C:1KG (clear water)
Step 2: A and B are mixed and churned together (churned together at high mechanical speed for about 3-4 minutes).
Step 3: AB content is high, after mixing, it is thicker and more viscous, so it is not convenient for brushing. You can according to the situation directly can add water to dilute to the appropriate viscosity, the normal recommendation can increase the weight rat
Shenzhen Jitian Chemical Co.,Ltd-Waterborne Epoxy Resin and Curing Agent | |||
Item | Water-based epoxy resin | Item | Water-based epoxy curing agent |
Appearance | Light yellow transparent liquid | Appearance | White transparent uniform liquid |
Epoxy equivalent (G/EQ) | 180-190 | Amine value | 230±30 |
Rotational Viscosity | 6000±2000 | Rotational Viscosity | 11000-15000 |
Solid content | 60±2 | Solid content | 60±2 |
Specific Gravity | 1.01-1.08 | Specific Gravity | 1.01-1.08 |
Ratio | Waterborne epoxy resin: waterborne curing agent=3:1 | ||
Shenzhen Jitian Chemical Co.,Ltd-Waterborne Epoxy Resin and Curing Agent | |||
Item | Water-based epoxy resin | Item | Water-based epoxy curing agent |
Appearance | Light yellow transparent liquid | Appearance | White transparent uniform liquid |
Epoxy equivalent (G/EQ) | 180-190 | Amine value | 230±30 |
Rotational Viscosity | 6000±2000 | Rotational Viscosity | 11000-15000 |
Solid content | 60±2 | Solid content | 60±2 |
Specific Gravity | 1.01-1.08 | Specific Gravity | 1.01-1.08 |
Ratio | Waterborne epoxy resin: waterborne curing agent=3:1 | ||