Polymerized rosin is processed by advanced new technology of sulfuric acid-zinc chloride method, with high dimer content, light color, high softening point, no crystallization, high acid value, low content of hot water solubles, good oil solubility, discoloration of lead acetate Lighter and softer than rosin.
Shenzhen Jitian Chemical Co., Ltd.-Polymerized Rosin | ||||
Product brand index | B-90 | B-115 | B-140 | |
Exterior | Transparent | Transparent | Transparent | |
colour | Glass color is lighter than or equal to | Level 4 | Level 3 | Level 3 |
The sodium color is lighter than or equal to | April 6 | April 6 | April 6 | |
Softening Point | 90-100 | 110-120 | 135-145 | |
Acid value, mgKOH / g≥ | 165 | 145 | 140 | |
Ethanol insoluble matter (%) ≤ | 0.03 | 0.03 | 0.03 | |
Hot water solubles (%) ≤ | 0.2 | 0.2 | 0.2 | |
Note: The above data is for reference only, the actual personal experiment shall prevailNote: The above data is for reference only, the actual personal experiment shall prevail | ||||
Shenzhen Jitian Chemical Co., Ltd.-Polymerized Rosin | ||||
Product brand index | B-90 | B-115 | B-140 | |
Exterior | Transparent | Transparent | Transparent | |
colour | Glass color is lighter than or equal to | Level 4 | Level 3 | Level 3 |
The sodium color is lighter than or equal to | April 6 | April 6 | April 6 | |
Softening Point | 90-100 | 110-120 | 135-145 | |
Acid value, mgKOH / g≥ | 165 | 145 | 140 | |
Ethanol insoluble matter (%) ≤ | 0.03 | 0.03 | 0.03 | |
Hot water solubles (%) ≤ | 0.2 | 0.2 | 0.2 | |
Note: The above data is for reference only, the actual personal experiment shall prevailNote: The above data is for reference only, the actual personal experiment shall prevail | ||||