Chlorinated rubber is widely used in coatings, inks and adhesives for its excellent wear resistance, adhesion, water permeability resistance, quick drying, flame retardancy and corrosion resistance.
Appearance: white particles or powder
Chlorine content (%): ≥65
Viscosity (20% xylene solution 25 ℃) mpa.s: 30-50
Volatile (%): ≤0.6
Stability: It is stable at atmospheric room temperature, but a slow degradation reaction will occur during continuous heating. It is recommended to add low molecular weight epoxy resin as a stabilizer during the production process.
Compatibility: Compatible with most plasticizers. The most commonly used is chlorinated paraffin. For example, 52 ° chlorinated paraffin, according to different requirements for coating, the recommended ratio of chlorinated rubber to chlorinated paraffin is 2-3.5: 1. In addition, it is compatible with alkyd and acrylic resins.
Appearance: white particles or powder
Chlorine content (%): ≥65
Viscosity (20% xylene solution 25 ℃) mpa.s: 30-50
Volatile (%): ≤0.6
Stability: It is stable at atmospheric room temperature, but a slow degradation reaction will occur during continuous heating. It is recommended to add low molecular weight epoxy resin as a stabilizer during the production process.
Compatibility: Compatible with most plasticizers. The most commonly used is chlorinated paraffin. For example, 52 ° chlorinated paraffin, according to different requirements for coating, the recommended ratio of chlorinated rubber to chlorinated paraffin is 2-3.5: 1. In addition, it is compatible with alkyd and acrylic resins.
Product introduction
Chlorinated rubber is widely used in coatings, inks and adhesives for its excellent wear resistance, adhesion, water permeability resistance, quick drying, flame retardancy and corrosion resistance.
Typical Properties
Appearance: white particles or powder
Chlorine content (%): ≥65
Viscosity (20% xylene solution 25 ℃) mpa.s: 30-50
Volatile (%): ≤0.6
Stability: It is stable at atmospheric room temperature, but a slow degradation reaction will occur during continuous heating. It is recommended to add low molecular weight epoxy resin as a stabilizer during the production process.
Compatibility: Compatible with most plasticizers. The most commonly used is chlorinated paraffin. For example, 52 ° chlorinated paraffin, according to different requirements for coating, the recommended ratio of chlorinated rubber to chlorinated paraffin is 2-3.5: 1. In addition, it is compatible with alkyd and acrylic resins.
Application/Uses
Chlorinated rubber is one of the chlorinated polymers obtained by chlorination modification of natural rubber or synthetic rubber. Due to its excellent film forming, adhesion, corrosion resistance, flame retardancy and insulation, it can be widely used in the manufacture of adhesives, marine paints, container paints, chemical anticorrosive paints, road marking paints, fireproof paints, and construction Paints and printing inks are one of the promising chlorine-based fine chemical products.
Comments
Properties reported here are typical of average lots. Jitian chemical makes no representation that the material in any particular shipment will confirm exactly to the values given.
Packaging and storage:
20KG per pack. Store in a dry environment at room temperature. This product is non-dangerous and has stable chemical properties.
REMARK |
Jitian Chemical shall not be responsible for the use of this information, or of any product, method, or apparatus mentioned, and you must make your own determination of its suitability and completeness for your own use, for the protection of the environment , and for the health and safety of your employees and purchasers of your products. No warranty is made of the merchantability of fitness of any product and nothing herein waves any of the seller's conditions of sale
|

Copy product links
Long by picture save/share

+86 15986601598
+86 15817282250
(+86) 755-88834518
Monday to Friday: 9:00-18:00